This article is from Dental Research Journal , volume 9 . Abstract Background:: Antioxidizing agents have recently been suggested to compensate decreased bond strength of resin materials to bleached tooth tissues. This study compared the shear bond strength (SBS) of three different adhesives on bleached dentin immediately after bleaching, bleached/delayed for 1 week, and bleached/applied antioxidizing agent. Materials and Methods:: The dentinal surfaces of 132 intact extracted molars were prepared and divided into 12 groups. The following adhesives were investigated: Optibond FL (OFL) (three-step etch-and-rinse), Optibond Solo Plus (two-step etch-and-rinse), and Optibond all-in-one (OA) (one-step self-etch) (Kerr, Orange, USA). Unbleached dentin groups (groups 1-3) were prepared as negative controls (NC). The remainder surfaces (groups 4-12) were bleached with 20% Opalescent PF (Ultradent, USA). Specimens were bonded immediately after bleaching (groups 4-6), after 1 week (groups 7-9), or after using 10% sodium ascorbate (SA) gel (groups 10-12). Subsequent to bonding of composite resin, the samples were tested for SBS and analyzed using Kruskal-Wallis and Mann-Whitney tests (α=0.05)
Sign in with your free account to read, download EPUBs or listen.
Ebook · Post-bleaching application of an antioxidant on dentin bond strength of three dental adhesives. · Khoroushi, Maryam, Saneie, Tahereh · Internet Archive