This article is from Contemporary Clinical Dentistry , volume 3 . Abstract Aims and Objectives:: To compare the marginal sealing ability of ormocer with a hybrid composite using an ormocer based bonding agent and a conventional fifth generation bonding agent. Materials and Methods:: Fifty four human premolars were randomly distributed into four test groups of 12 teeth each and two control groups of 3 teeth each. Class I occlusal preparation of 1.5 mm depth were made in each tooth. These were restored using the adhesive and restorative material according to the group. The restorations were finished using a standard composite finishing and polishing kit. Thermocycling between 5° C and 55°C was carried out. Having blocked the root apex and the entire tooth surface except 1 mm around the restoration margin, the teeth were immersed in 2% methylene blue for 48 hours, after which the dye penetration through the margins of each sample was studied under a stereomicroscope. Results and Discussion:: Group IV (Admira with Admira Bond) showed the minimum marginal leakage with a mean of 0.200 mm. Four samples in this group showed no microleakage at all and a maximum of 0.400 mm was seen in one s
Sign in with your free account to read, download EPUBs or listen.
Ebook · Ormocer: An aesthetic direct restorative material; An in vitro study comparing the marginal sealing ability of organically modified ceramics and a hybrid composite using an ormocer-based bonding agent and a conventional fifth-generation bon · Kalra, Sarika, Singh, Arundeep, Gupta, Manish, Chadha, Vandana · Internet Archive